Our Tests

  • Tensile Strength (MPa)
  • Elongation at Break (%)
  • Hardness (IRHD)
  • Hardness (Shore A)
  • Yırtılma Dayanımı  (kN / m)
  • Compression Set (%)
  • Accelerated Ageing (change in hardness after ageing) (Shore A and IRHD)
  • Accelerated Ageing (change in tensile strength after ageing) (%)
  • Accelerated Ageing (change in elongation at break after ageing) (%)
  • Low Temperature Resistance
  • Ageing in Liquids (%)
  • Volume Change in Water (%)
  • Abrasion Resistance (%)
  • Spesific Gravity (g/cm³)
  • Rheometer
  • Viscometer
  • Moisture Measurement (%)
  • Stress Relaxation (%)
  • Ash Content (%)
  • Load-Deflection Test (kN/mm)
  • Compression Stiffness (kN/mm)
  • Shear Modulus (MPa)
  •  Shear Bond
  • Project Proof Load Test (kN/mm)
  • Water Tightness for Tunnel Segment Gaskets (Bar)